This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2015, 6, 2224–2232, doi:10.3762/bjnano.6.228
Figure 1: (A, B) SEM micrographs of the surface morphology of a gold substrate deposited at 100 Pa in Ar with...
Figure 2: (A) SERS spectra of 100 µg/mL APO (dipping time: 5 min) collected with different exposure times on ...
Figure 3: SERS of APO solutions at four different concentrations (100, 10, 1, 0.1 µg/mL; dipping time 5 min; ...
Figure 4: Peak areas (baseline-corrected) plotted against the concentration of APO solutions that summarize t...
Figure 5: Effect of the dipping time on the dynamic range of the APO concentration of the gold sensor. Linear...
Figure 6: APO crystal growth on the gold sensor (dipping time 10 min). The scattered data result when plottin...
Figure 7: SERS spectra of unfiltered blood plasma with (A) APO 200 µg/mL, and (B) APO 20 µg/mL. SERS spectra ...